RussianPatents.com

Sintered electro-contact material on base of copper. RU patent 2415958.

FIELD: metallurgy.

SUBSTANCE: sintered electro-contact material on base of copper contains, wt %: soot of zinc oxide - 2.2 - 2.5; aluminium - 0.001 - 0.005; tungsten - 3 - 10; copper - the rest.

EFFECT: high hardness, density and low intensity of wear.

2 tbl, 1 ex

 


 

IPC classes for russian patent Sintered electro-contact material on base of copper. RU patent 2415958. (RU 2415958):

H01H1/025 - Electric switches
C22C9 - Alloys based on copper
C22C1/05 - ALLOYS (treatment of alloys C21D, C22F)
Another patents in same IPC classes:
Domestic device and methods of its control Domestic device and methods of its control / 2406177
According to the present invention, one version of domestic device implementation includes control panel and controller. The control panel may contain electric switch, which can be utilised by the user to supply commands for device energising and de-energising, and input unit for supplying commands for device actuation by the user.
Method of producing powder ceramet cu-cd/cdo for electric contacts / 2401314
Mix material is prepared containing powders of copper and cadmium with the solution of thermally unstable cadmium salt. Said mix is dried and thermally treated at 300-500°C. Produced burden is subjected to cold briquetting and sintering. Then second compaction and annealing are performed to produce Cu-Cd/CdO.
Composite electric contact and method of its fabrication / 2400852
Proposed contact is made from graphite-based material containing metal additives. Note here that graphite base is made from fine-grained busy graphite with specific resistance of not over 16 mcmOhm*m, compression strength making at least 60 MPa, ash content not exceeding 0.3% and bulk porosity of 15-25%. Metal additive is distributed in graphite pores in amount making at least 10% of pore volume, while metal additive particles form discontinuous 10 mcm-thick surface coat on graphite base surface. Proposed method involves mechanical dimensional processing of contact made from structural graphite, impregnating said contact with ethanol and holding it in water solution of silver nitrate of density varying from 1.4 to 1.17 g/cm3 at temperature 10-40°C higher than boiling temperature of impregnation liquid during 10-15 min. Then contact is subjected to thermal treatment at below 0.95 of silver melting temperature for 0.5-1.0 h, said contact being placed in container and backfilled by char coal.
Method of producing composite material for copper-based electric contacts Method of producing composite material for copper-based electric contacts / 2398656
Invention relates to powder metallurgy, particularly to method of producing copper-based composite materials. It can be used for production of electric contacts. Powders of graphite, copper, aluminium, phosphor copper and copper oxide are mixed at the following ratio, wt % graphite 0.10-0.20; aluminium 0.20-0.30; phosphor copper 0.05-0.15; copper oxide 1.15-1.4; copper making the rest. Prepared mix is subjected to high-power treatment in ball mill to produce granules of material representing copper-based matrix with reinforcing particles uniformly distributed therein in amount of 0.35 to 0.55 wt % of total weight with average size of 0.1 to 0.5 mm. Material matrix represents α-Cu(Al) substitutional solution while reinforcing particles - γ-Al2O3 with average size of 20-40 nm. Mix is compacted by extruding in heated state.
Multi-layer electric contact Multi-layer electric contact / 2381587
Invention relates to electrical engineering, particularly to the design of multi-layer electric terminal operated at higher temperatures. Proposed terminal comprises temporary nickel layer, intermediate silver layer and surface layer made from refractory iron-aluminium-based alloy with aluminium content not over 5%, from "Х27Ю5Т" alloy that allows aluminium diffusion onto terminal surface and transition into oxide, oxide film thickness varying from 5 nm to 30 nm.
Material for high-current sliding electrocontact / 2368971
Invention relates to powder metallurgy, particularly to antifriction materials. It can be used for manufacturing of current-collecting brush, particularly homopolar generators or current-collecting shoes, contacting to rail. Composite material of following composition, wt %: copper 18-46; graphite 2-3; treated steel "ШХ15" - the rest.
Composite material of contact plate on copper basis and method of its manufacturing / 2368462
Invention can be used for manufacturing of contact members of current collectors of electric motive power of railroads, municipal and industrial transport. Composite material contains components in a following ratio, wt %: graphite - 3.0-10.0, iron - 7.0-10.0, phosphorus - 0.1-0.5, sulphur - 0.1-0.8, age-hardened copper- the rest. Manufacturing method of composite material includes manufacturing of age-hardened copper, containing 0.3-4.5 wt % age-hardening additives, mixing of powder materials, compressing from them porous blank, heating of compressed blank, its compaction and cold hardening of the received material.
Metal-oxide material for bursting electric contacts / 2367695
Metal-oxide material consists of metallic substrate in the form of silver or copper and oxide component - cadmium stannate in amount 10-15 wt %.
Metal-oxide material for bursting electric contacts / 2367695
Metal-oxide material consists of metallic substrate in the form of silver or copper and oxide component - cadmium stannate in amount 10-15 wt %.
Sliding contactor of automatic circuit-breaker Sliding contactor of automatic circuit-breaker / 2343582
Invention is attributed to sliding contactor of automatic circuit-breaker. Sliding contactor of automatic circuit breaker comprises: body; multiple pins located on the body; side plate with axis and certain area having axial portion protruding from one of its sides for certain length and connected with both body side surfaces thus covering the pins; and buckle connected with load side junction terminal linked with fixed contactor, for entering with possibility to rotate the section with axis integrated with side plate axis.
Copper-zinc alloy, and baulk ring of synchroniser made out of this alloy Copper-zinc alloy, and baulk ring of synchroniser made out of this alloy / 2415188
Here is claimed copper-zinc alloy, its application for fabrication of baulk ring of synchroniser and baulk ring of synchroniser. Alloy contains from 55 to 75 wt % of copper, from 1.65 to 8 wt % of aluminium, from 0.3 to 3.5 wt % of iron, from 0.5 to 8 wt % of manganese, from 0 to less 5 wt % of nickel, from 0 to less 0.1 wt % of lead, from 0 to 3 wt % of tin, from 0.3 to 5 wt % of silicon, from 0 to less 0.1 wt % of cobalt, from 0 to less 0.05 wt % of titanium, from 0 to less 0.02 wt % of phosphorus, unavoidable impurities, and zinc - the rest.
Procedure for production of composite material on metal matrix reinforced with quazi-crystals / 2413781
Invention can be implemented for fabrication of parts of friction units operating at temperature up to 600°C used in aircraft, ship building, automobile and other branches of industry. Powder of quazi-crystals Al-Cu-Fe is placed into a press-mould, is soaked with melt of tin or lead at temperature 300-400°C and pressure not over 400 MPa and crumbled. Produced powder is mixed with powder of copper matrix, is pressed and thus produced mixture is extruded.
Copper alloy cu-si-co for materials of electronic techology and procedure for its production Copper alloy cu-si-co for materials of electronic techology and procedure for its production / 2413021
Copper alloy for materials of electronic technology consists from 1.0 to 2.5 wt % Ni, from 0.5 to 2.5 wt % Co and from 0.30 to 1.2 wt Si, the rest is copper and unavoidable impurities. Median value ρ is 20-60 wt %, mean square deviation is σ (Ni+Co+Si) ≤30 wt %, share of area of surface of particles of the second phase S of dimension 0.1 mcm or more and 1 mcm or less observed in cross section parallel to direction of rolling is 1-10 %.
Bronze for heat exchanging equipment and protective systems of nuclear reactors Bronze for heat exchanging equipment and protective systems of nuclear reactors / 2412268
Bronze contains, wt %: chromium 0.4-1.2, zirconium 0.1-0.5, vanadium 0.1-0.5, nickel 0.15-0.25, aluminium 0.05-0.15, beryllium 0.03-0.1, yttrium 0.01-0.05, copper - the rest. Summary contents of chromium and vanadium does not exceed 1.5 wt %.
Composite sintered powder material / 2405848
Composite sintered powder material contains copper powder with grain size of 100-160 mcm, granules of copper-plated graphite with grain size of 160-200 mcm in quantity of 16-17 wt % at copper content in granules of copper-plated graphite of 70-75 wt %, granules of copper-plated polymer with grain size of 50-200 mcm in quantity of 7-9 wt % at copper content in granules of copper-plated polymer of 50-60 wt %, granules of copper-plated nickel with grain size of 100-200 mcm in quantity of 3-5 wt % at copper content in granules of copper-plated nickel of 25-35 wt %, granules of copper-plated chrome with grain size of 25-75 mcm in quantity of 6-8 wt % at copper content in granules of copper-plated chrome of 30-40 wt %, carbon nano-tubes in quantity of 0.2-0.7 wt % and fullerenes in quantity of 0.02-0.04 wt %.
Tin bronze for consumable electrodes of plate roller electric-discharge texturing machines Tin bronze for consumable electrodes of plate roller electric-discharge texturing machines / 2401315
Proposed invention can be used in producing rod consumable electrodes of plate roller electric-discharge texturing machines. Bronze contains the following components, in wt %: tin 4.0-less that 6.0, phosphorus 0.1-0.3, antimony not over 0.002, silicon not over 0.002, iron not over 0.05, copper making the rest.
Method of producing powder ceramet cu-cd/cdo for electric contacts / 2401314
Mix material is prepared containing powders of copper and cadmium with the solution of thermally unstable cadmium salt. Said mix is dried and thermally treated at 300-500°C. Produced burden is subjected to cold briquetting and sintering. Then second compaction and annealing are performed to produce Cu-Cd/CdO.
Copper-based alloy / 2400554
Copper-based alloy contains the following, wt %: stannum 5.0-7.0; zinc 8.0-8.5; titanium 0.001-0.002; tungsten 0.03-0.08; zirconium 0.01-0.02; nickel 0.3-0.4; silver 0.9-1.3; copper - the rest.
Copper-based alloy / 2400554
Copper-based alloy contains the following, wt %: stannum 5.0-7.0; zinc 8.0-8.5; titanium 0.001-0.002; tungsten 0.03-0.08; zirconium 0.01-0.02; nickel 0.3-0.4; silver 0.9-1.3; copper - the rest.
Wear-resistant composite powder material on copper base for contact plates of current collectors of electric stock Wear-resistant composite powder material on copper base for contact plates of current collectors of electric stock / 2400550
Invention can be used for production of contact plates of current collectors of electric stock of railway transport. Wear-resistant composite powder material on copper base includes the following, wt %: iron 0.5-10; graphite 6.0-8.0; stannum 0.5-7.0; phosphorus 0.3-0.4; cast iron 2.78-5.97; copper - the rest. At that, cast iron is in the form of disperse secondary phase equally distributed in copper particles in quantity of 3-8 wt % of secondary phase with average size of 0.05-11 mcm.
Precision alloy Precision alloy / 2415189
Here is claimed precision alloy for die casting and procedure for its production. Alloy contains aluminium 42 wt % or more and 45 wt % or less, silicon 2 wt % or more and 8 wt % or less. The procedure for ally production consists in production of melt containing aluminium, zinc, silicon, copper and magnesium and in production of precision alloy for die casting containing in terms of total weight 42 wt % or more and 45 wt % or less of aluminium, 30 wt % or more and 57.89 wt % or less of zinc, 2 wt % or more and 8 wt % or less of silicon, 0.1 wt % or more and 0.2 wt % or less of copper, 0.01 wt % or more and 0.1 wt % or less of magnesium and unavoidable impurities.
© 2013-2014 Russian business network RussianPatents.com - Special Russian commercial information project for world wide. Foreign filing in English.