Method of manufacturing cellulose-polymer composites

FIELD: polymer materials in paper-and-pulp industry.

SUBSTANCE: invention relates to manufacturing cellulose-polymer composites that can be, in particular, used in production paper or cardboard. Method according to invention providing a composition and manufacturing sheet therefrom followed by drying. In the method of invention, aqueous nanodispersion of polyorganosiloxanes is utilized, which can be introduced into composition or can be deposited onto sheet before drying on size press or after drying of sheet to moisture content not less than 12°.

EFFECT: improved waterproofness, increased inflammation temperature, and improved physicochemical characteristics of material.

4 cl

 

The present invention relates to technology for cellulose-polymer composite materials and can be used in various industries, such as woodworking, chemical, chemical, pulp and paper industry, for example, in the manufacture of many types of paper or cardboard.

Closest to the claimed solution is a method of manufacturing a cellulose-polymer composites, in which the composition is prepared with the subsequent manufacturing of the fabric, followed by drying and processing, as well as possible by recycling, using organosilicon compounds, such as NGL-94 (see SU # 107429, CL D21H 21/16, epubl).

The main disadvantage of the known solutions is a significant pozarovzryvobezopasnost process due to the use of organic solvents for the introduction of organosilicon compounds.

The technical result of the proposed method is to increase the hydrophobicity, increasing the ignition temperature, the improvement of physical and mechanical properties of the material.

This technical result is achieved by a method of manufacturing a cellulose-polymer composite materials, including composing, production of her paintings followed his suck the th, this use of organosilicon compounds in aqueous nanodispersions of polyorganosiloxanes. Nanodispersion of polyorganosiloxanes you can enter in composition, put on canvas paper before drying or after drying.

The invention is illustrated by the following examples.

Example 1.

A method of manufacturing a cellulose-polymer composite materials, such as cardboard weighing 150 g/m

In the composition of the waste paper grades MS-6, MS-7 before forming enter polyorganosiloxanes on TU-2310-001-18 803089-2002 in aqueous nanodispersions in an amount of about 60 kg/t of waste paper. Produce sheen of the fabric, followed by drying on the paperboard machine. Drying is carried out at a temperature of at least 105°on the drying drums with the use of ultraviolet radiation.

You get gidrofobiziruyuschey coating film without effect, providing strong protection from moisture environment.

Example 2.

The method is carried out analogously to example 1. The only difference is that as cellulose-polymer composite material was obtained sack paper wet-strength weight 90 g/m2of bleached sulphate pulp. Water nanodispersion of polyorganosiloxanes on TU-2310-001-18803089-2002 in an amount of about 60 kg/t of sulphate pulp is applied to the cloth before drying at the size press is E.

Get gidrofobiziruyuschey coating film without effect, providing strong protection from moisture environment.

Example 3.

The method is carried out analogously to example 1. The only difference is that as cellulose-polymer composite materials are made of wood-fiber Board marks M-1 density of 350 kg/m3wood fiber. On the cloth after dry pressing cause water nanodispersion of polyorganosiloxanes on TU-2310-001-18 803089-2002 in an amount of about 85 kg/t of raw wood.

Get gidrofobiziruyuschey coating film without effect, providing strong protection from moisture environment.

This way you can get a paper, cardboard, fibreboard, etc.

In is used as raw material refined and highly plasticised cellulose, wood pulp and waste paper.

Thus, the invention improves the degree of hydrophobization by volumetric effects on cellulose-polymer composite materials. This significantly reduces the use of environmentally harmful substances and provide a broad technological capabilities.

Allows you to create a fundamentally new cellulose-polymer composite materials.

The proposed method is simple to implement and does not require specially what about the equipment.

1. A method of manufacturing a cellulose-polymer composite materials, including composing, production of her paintings with subsequent drying, while the use of organosilicon compounds in aqueous nanodispersions of polyorganosiloxanes.

2. The method according to claim 1, in which the water nanodispersion of polyorganosiloxanes enter into the composition.

3. The method according to claim 1, in which the water nanodispersion of polyorganosiloxanes put on a cloth to dry.

4. The method according to claim 1, in which the water nanodispersion of polyorganosiloxanes applied to the fabric after drying.



 

Same patents:

FIELD: pulp-and-paper industry; methods of production of the laminated paper of the high density and the high oxygen permeability.

SUBSTANCE: the invention is pertaining to the field of the pulp-and-paper industry, in particular, to the barrier substance and the method of its realization. The method allows to produce the laminate of the paper coated with the polyolefin, at that the paper is manufactured out of the wet fibrous mass, which is not enabled to dry before manufacture of the paper, and before the polyolefin application on the paper - the paper is modified in such a manner that its surface energy has changed approximately up to the value equal to the surface energy value of the polyolefin. The presented method ensures the manufacture of the barrier substance with the stable quality and the good barrier properties with respect to the gas and may be used for packaging, in particular, for the food products.

EFFECT: the invention ensures the manufacture of the barrier substance with the stable quality and the good barrier properties with respect to the gas and may be used for packaging, in particular, for the food products.

12 cl, 5 dwg, 4 tbl, 3 ex

FIELD: pulp-and-paper industry, in particular, manufacture of paper which may be used for hygienic and household purposes.

SUBSTANCE: paper sheet consists of at least two layers of creped cellulose wool, upper and lower layers, said layers having weight within the range of 10-40 g/m2. Upper layer is embossed and equipped with primary projections divided along lines defining therebetween cells with surface within 1-20 cm2. Upper layer has longitudinal length exceeding that of lower layer by at least 0.6%, preferably by 0.6-2%, and is connected with said lower layer through apexes of primary protrusions so that pads are defined within cells. Method involves unwinding first band of cellulose wool from main bobbin; performing embossments on roll for providing embossment in accordance with pattern including primary projections forming lines which define closed cells therebetween; unwinding second band of cellulose wool from main bobbin; applying second band onto first band and connecting both bands through apexes of primary projections; winding resultant doubled band onto cartridge while applying tensile force; differentiating both bands in the process of joining so that at rest state length of both layers differs by at least 0.6%, preferably 0.6-2%; cutting resultant roll into smaller rolls.

EFFECT: increased convexity effect for simulating textile product.

10 cl, 3 dwg

FIELD: paper coated with composition for coating various kinds of paper, for offset printing of paper used for manufacture of books, magazines, annual reports, or packaging paper.

SUBSTANCE: composition comprises pigments and binder. Composition pigments are formed as microballs having sizes below 10 micrometers, preferably about 7 micrometers. Paper coated with such composition is silky by touch and has at least one surface coated with such composition, preferably both of its surfaces. This paper may be tracing paper.

EFFECT: improved quality of paper owing to preventing sliding thereof during separation of sheets in stacks, delamination of coating during printing process and, accordingly, elimination of paper dusting and formation of impure imprints.

7 cl, 2 dwg, 2 tbl, 13 ex

FIELD: cellulose-paper industry.

SUBSTANCE: device for continuous connection of paper sheets contains means useable to press aforementioned sheets 5,6 on printing cylinder or shaft 4, simultaneously moving sheets to outlet section of device. Aforementioned means for pressing contains shaft or cylinder 2 provided with rigid external surface, supported by elastic surface positioned below it. Method for connecting two sheets of paper 5,6 contains stage of pressing of sheets between pressing shaft or cylinder 2, provided with rigid external surface and elastic surface positioned below it, and printing cylinder or shaft 4, provided with relief and/or recesses across the surface.

EFFECT: increased quality due to prevention of unwanted deformations of surface of connected sheets, simple manufacture, economic efficiency, extensive service life.

2 cl, 23 dwg

FIELD: investigating or analyzing materials.

SUBSTANCE: paper comprises paper matrix that contains organic reagent made of aluminon. The paper matrix is made of cellulose modified by epichlorohydrin. The organic reagent is made of a composition of adsorbed aluminon with covalently immobilized aluminon. The cellulose modified by epichlorohydrin is related to adsorbed aluminon and is related to covalently immobilized aluminon as (500-1000):(5-9):1, in mass.

EFFECT: enhanced reliability of determining.

7 dwg, 3 tbl, 4 ex

FIELD: paper and pulp industry.

SUBSTANCE: method comprises applying glue at least on the first layer by passing the first layer between the counter-pressing cylinder and roller for batching glue, setting the second layer in the region of the first layer and in the contact with the glue applied on the first layer, and gluing the first layer to the second layer between the counter-pressing cylinder and gluing roller. The glue is applied in the zones of projecting bosses provided on the glue batching roller . The density and sizes of the bosses are chosen to provide sufficient amount of glue between two layers. The device comprises counter-pressing roller provided with a number of bosses and engaging the batcher of glue, pressing roller, and gluing roller.

EFFECT: enhanced adhesion.

40 cl, 8 dwg

FIELD: pulp-and-paper industry, in particular production of multilayered cellulose product preferably paper or paperboard.

SUBSTANCE: claimed method includes filler application between at least two layers of moving fibrous material before bonding thereof with one another. In preferable embodiment inorganic filler is used optionally containing organic components. In the most preferable embodiment calcium sulfate is used.

EFFECT: paper with better optical characteristic such as whiteness and opacity without losses of mechanical properties.

42 cl, 7 dwg

Toilet paper // 2275836

FIELD: production of sanitary and hygienic articles.

SUBSTANCE: toilet paper according to one version has paper base containing substance effectively acting upon skin of anal and perianal regions. Conjugate acid-base pair used as said substance is adapted for forming upon contacting with skin of anal and perianal regions of buffer system with pH of from 4.5 to 6.0, said system being composition containing weak acid and weak acid salt with strong base, or weak base and strong base salt with weak base or combination of acid salts. Toilet paper according to other version includes paper base containing active components of medicinal drugs. Paper base additionally contains composition of weak acid and weak acid salt with strong base or of weak base and strong acid salt with weak base or of weak base and strong acid salt with weak base, or combination of acid salts. Said composition provides, upon contacting with skin of anal and perianal regions, pH value of said skin in the range of from 4.5 to 6.0.

EFFECT: increased hygienic, curative and prophylactic efficiency of toilet paper.

3 cl

FIELD: paper industry.

SUBSTANCE: base paper for decorative coating materials contains 10 to about 65% of pigment, which includes silicon- and aluminum-modified titanium dioxide in combination with another, white pigment. Titanium dioxide-based pigment is characterized by oil capacity at least 25% and solubility in sulfuric acid at least 15% TiO2. Invention also provides decorative paper or decorative film containing above base paper.

EFFECT: increased opacity of base paper at lower consumption of titanium dioxide.

7 cl, 1 tbl, 8 ex

FIELD: paper industry.

SUBSTANCE: base paper for decorative coating materials contains 10 to about 65% of pigment, which includes silicon- and aluminum-modified titanium dioxide in combination with another, white pigment. Titanium dioxide-based pigment is characterized by oil capacity at least 25% and solubility in sulfuric acid at least 15% TiO2. Invention also provides decorative paper or decorative film containing above base paper.

EFFECT: increased opacity of base paper at lower consumption of titanium dioxide.

7 cl, 1 tbl, 8 ex

The invention relates to a method of reducing residue from the combustion of paper or paperboard coated, to a method of reducing wear of the grid used in the production of paper or cardboard, fibrous roll material coated

The invention relates to an agent that increases the strength of paper in the wet state, and the method of its production, and method for producing a paper containing this agent

The invention relates to mixtures of cationic starch with a cationic galactomannan gum, such as husarova gum, gum carob, fenugreek, Greek, etc. that can be used as a means that can help give strength and dehydration in the manufacture of paper

The invention relates to the pulp and paper industry, in particular the production of separator paper, which will find application in electrical industry for chemical current sources with an alkaline electrolyte

The invention relates to the pulp and paper industry

The invention relates to the production of multi-layer waterproof paper and can be used in the pulp and paper industry for paper production for the major layers of decorative paper laminate (DBSP)

The invention relates to the production of multi-layer paper and can be used in the pulp and paper industry for paper production for the major layers of decorative paper laminate

The invention relates to the pulp and paper industry, in particular to methods of producing paper for the inner layers of decorative paper laminates containing phenol-formaldehyde resin

FIELD: paper-and-pulp industry.

SUBSTANCE: cellulose product contains clay having stacking of atomic planes 2R2. Product represents paper of fibrous pulp, while clay has cationic nature. Preparation of product comprises: providing aqueous suspension containing cellulose fibers and optionally filler; adding clay having stacking of atomic planes 2R2.to suspension; and dehydrating thus prepared suspension. Another method of preparing cellulose product comprises: providing aqueous suspension containing cellulose fibers and optionally filler; adding cationic clay to suspension; adding one or several draining auxiliary substances enhancing retention of filler and containing at least one cationic polymer; and dehydrating thus prepared suspension.

EFFECT: reduced interfering and harmful substance in cellulose suspension and enhanced retention of filler, dehydrating agents, and sizing agents.

27 cl, 14 tbl, 13 ex

FIELD: food industry; packing.

SUBSTANCE: invention relates to packing material containing base paper or cardboard layer for packing container formed by bending and welding the sheet, or flat blank of packing material. Laminated packing material has base paper or cardboard layer and outer coatings from both sides of base layer made of thermoweldable polymer impermeable to liquids. Said paper or cardboard base layer is made water-repelling by sizing the mass by water dispersoid solution or emulsion of alkylketene dimer or mixture of alkylketene dimers so that content of alkylketene dimer (dimers)in base layer is from 0.25 to 0.4 by dry weight, weight %. Invention contains description of method of manufacture of laminated material and packing container to be sterilized.

EFFECT: provision of laminated packing material protected from penetration of hot steam or liquid designed for packing food products and capable of withstanding heat treatment in autoclave at high humidity and temperature without separation of packing material into layers.

6 cl, 2 dwg

FIELD: pulp-and-paper industry, in particular paper or board production.

SUBSTANCE: claimed method includes providing of slurry containing cellulose fiber and at least sizing agent interacting with cellulose. Sizing agent is selected from group containing ketene dimmers and acid anhydrides. Cationic vinyl polymer obtained by additional polymerization, containing aromatic units and anionic vinyl polymer obtained by additional polymerization and having molecular mass from 6000-100000 are introduced into slurry. Then obtained slurry is dehydrated and paper leaf is formed.

EFFECT: increased effectiveness of sizing, dehydration and retention.

11 cl, 3 tbl, 2 ex