Combined reagent for cement slurries

 

The invention relates to the fastening of oil and gas wells and can be used for bulk blending or cement slurries in the first place lightweight curing at low and moderate positive temperatures. Combined reagent for cement slurries, including aluminum sulfate, additionally contains aluminum hydroxide chloride, polyaluminium hydroxide chloride in the following ratio, wt.%: aluminum hydroxide chloride, polyaluminium hydroxide chloride 40-55, aluminum sulfate 45-60. The technical result - developing reagent, providing a stable technological properties of cement slurries regulating the dielectric strength and setting time. table 1.

The invention relates to the fastening of oil and gas wells and can be used for bulk blending or cement slurries in the first place lightweight curing at low and moderate positive temperatures.

A known solution on the basis of Portland cement and water, which includes an integrated reagent hydrochloric aluminum [1].

Combined reagent in this solution the Yu is the grouting composition, containing cement, additive-reagent and water, and in addition it contains a complex reagent, consisting of several components in the following ratios, wt.%: aluminum hydroxide 0,45-0,7; sodium aluminate - 0,9-1,5; aluminium sulphate - 0,45-0,7 [2].

The disadvantage of a complex of a reagent of the prototype is its lack of ability to provide a stable technological properties of the cement slurry.

The objective of the invention is to develop a reagent that provides a stable technological properties of cement slurries, especially lightweight, hardening at low and moderate temperatures.

The problem is solved in that the complex reagent for cement slurries, including aluminum sulfate, additionally contains aluminum hydroxide chloride, polyaluminium hydroxide chloride in the following ratio, wt.%: Aluminum hydroxide chloride, polyaluminium hydroxide chloride - 40-55 Aluminum sulfate 45-60 the Totality of the claimed features provides the reagent ability to control such properties of cement slurry as insulating ability, time setting, stability, sedimentation and uniformity.

That is), provides deformation properties of the cement stone. The introduction of the reagent ions SO42-in the claimed amount significantly increases the number of ettringite, the crystals of which are reinforced delevigne the slightly basic hydrosilicate and thereby significantly increase the rate of hydration of cement mortars, reducing the duration of the seizure.

Anions of strong acids Cl-and SO42-have a coagulating effect on the dispersion system and it provides integrated reagent ability to influence the properties of the cement slurry in the manner described above.

Combined reagent is prepared by mechanical mixing in the specified proportions of its constituent components. To the obtained reagent depending on the geotechnical conditions of the wells may be added known plasticizers, accelerators, and fluid loss in known quantities.

Example 1 Into the mixer with spout enter 6,0 kg of dry aluminum sulfate (TU 12966-85) and with constant stirring served 4.0 kg of dry aluminum hydroxide chloride, polyaluminium hydroxide chloride (TU 6-09-05-14-56-96). Mix the components within 20 minutes. The received complex reagent in Yo and test it according to the existing industrial standards and state Standards. As knitting take, for example, a lightweight cement containing 25% of the microspheres, for example, which is more indicative of the effectiveness of the obtained reagent.

The test results of cement slurry are presented in table 1 (experiment 1).

Example 2 Into the mixer with spout injected 4.5 kg of dry aluminum sulfate and with constant stirring served 5.5 kg of dry aluminum hydroxide chloride, polyaluminum hydroxide chloride. Mix the components within 20 minutes. The received complex reagent in the amount of 1% by weight of cement injected into the liquid mixing cement slurry. Prepare cement slurry and test it according to the existing industrial standards and state Standards. As knitting take, for example, a lightweight cement containing 30% of the microspheres.

The test results of cement slurry are presented in table 1 (experiment 2).

The table shows that at low positive temperatures lightweight cement mortars harden quickly enough, the deformation properties of cement stone rise.

Despite the diluted dispersion medium containing 1.0% reagent, water segregation remains zero. The solution sedimentation sustainable.

Sources in the Soberania

Combined reagent for cement slurries, including aluminum sulfate, characterized in that it additionally contains aluminum hydroxide chloride, polyaluminium hydroxide chloride in the following ratio, wt. %: Aluminum hydroxide chloride, polyaluminium hydroxide chloride - 40-55 Aluminum sulfate 45-60

 

Same patents:

The invention relates to the oil and gas industry and can be used for the repair and insulation works (RIRs) in the gas, gas condensate and oil wells in process of drilling and operation to restore pathogenetically lining, namely cement rings

The invention relates to the oil industry, in particular to polymer cement compositions intended for the isolation of zones of absorption and repair and insulation works in wells

The invention relates to the oil industry, in particular, compositions for water shutoff, restore the tightness of the annular space may be used to control seepage of oil layers in workover

The invention relates to the field of oil production, in particular to methods isolation of absorbing layers in the borehole, and can be used to eliminate areas of acquisitions in the repair of production and injection wells with low formation pressure, as well as the regulation of the profile of injection wells and isolation of water production in oil wells

The invention relates to the oil and gas industry, and in particular to methods for the recovery of casing tightness
Grouting mortar // 2211304
The invention relates to the field of construction, and in particular to compositions of cement slurries used mainly when performing waterproofing-fastening work of the foundations and basements of building structures by special technology
The invention relates to the oil and gas industry, in particular to methods isolation of water production in oil and gas wells until the mounting holes the production column

The invention relates to the fastening of oil and gas wells with abnormally low, namely dry cement mixtures

The invention relates to the field of oil and gas industry and can be used for the repair and insulation works well

FIELD: oil and gas production.

SUBSTANCE: invention relates to grouting mortars used for cementing casing pipes of gas, gas-condensate, and oil wells complicated by presence of formations with low hydraulic rupture pressure as well as presence of permafrost rocks. Light-weight grouting mortar contains 47.0-60.0% special-type cement, 6.6-11.8% clinoptilite as light-weight additive, and water. As a result, casing-pipe annulus incidents during boring and running wells are avoided owing to improved parameters of grouting cement, in particular increased sedimentation stability of mortar, dimensional stability and needed strength of cement stone at low positive and negative temperature in early hardening stages are achieved at simultaneous lowering of grouting mortar density.

EFFECT: improved performance characteristics of grouting mortar.

1 tbl

FIELD: oil and gas chambers construction.

SUBSTANCE: method includes pumping of portion of water-absorbing acryl polymer, exposure of it in a well, pumping of second portion of same polymer, tempered on fresh water with concentration 1-20%, buffer of fresh water dries up, and before and after pumping of second portion of water-absorbing polymer, tempered on hydrocarbon liquid with concentration 10-20%, buffer of hydrocarbon liquid is pumped in, besides, said 2-portion systems are pumped into well multiple times.

EFFECT: higher efficiency.

1 ex

FIELD: oil and gas production.

SUBSTANCE: invention provides grouting composition intended for selective insulation of water inflows into wells, including those occurring under low-temperature and high-permeation oil reservoirs, as well as for suppressing lost-circulating zones and brine inflow zones. Composition including product of hydrolytic etherification of chlorine-containing phenyltrichlorosilane still residues with aqueous alcohol solution contains, more specifically, product obtained by hydrolytic etherification of 100 wt parts of indicated residues with 10-32,8 wt parts of 90-93% aqueous alcohol solution in presence of 10-40 wt parts of orthosilicic acid ethyl ester and, additionally, 15-35 wt parts of chlorine-containing phenyltrichlorosilane still residues at summary content of the two components 133.2-161.6 wt parts. Grouting composition may further contain up to 16.8 wt parts of polar solvent.

EFFECT: lowered repair operation cost, enabled utilization in a wide formation temperature range, including that in high-permeation and low-temperature oil reservoirs, and prolonged shelf time of grouting composition.

2 cl, 1 tbl

FIELD: oil extractive industry.

SUBSTANCE: method includes pumping, in carrying liquid - waterless mixture of oil products containing waterless oil, of powder-like water-soluble polymer and connector in amount of 0.05-0.2% for mass of carrying liquid or 30-100% for mass of power-like water-soluble polymer, as said mixture a mixture of waterless oil and light oil products processed in relation 0.1:9.9-9.9:0.1 is used, and as connector - dry aluminum nitrate, chrome nitrate, iron nitrate, magnesium nitrate, barium nitrate, calcium nitrate or their mixtures.

EFFECT: higher efficiency.

2 tbl

FIELD: oil extractive industry.

SUBSTANCE: method includes pumping, in carrying liquid - waterless mixture of oil products containing waterless oil, of powder-like water-soluble polymer and connector in amount of 0.05-0.2% for mass of carrying liquid or 30-100% for mass of power-like water-soluble polymer, as said mixture a mixture of waterless oil and light oil products processed in relation 0.1:9.9-9.9:0.1 is used, and as connector - dry aluminum acetate, chrome acetate, iron acetate, magnesium acetate, copper acetate, barium acetate, manganese acetate, calcium acetate or their mixtures.

EFFECT: higher efficiency.

1 tbl

FIELD: oil extractive industry.

SUBSTANCE: method includes pumping, in carrying liquid - waterless mixture of oil products containing waterless oil, of powder-like water-soluble polymer and connector in amount of 0.05-0.2% for mass of carrying liquid or 30-100% for mass of power-like water-soluble polymer, as said mixture a mixture of waterless oil and light oil products processed in relation 0.1:9.9-9.9:0.1 is used, and as connector - dry aluminum sulfate, chrome sulfate, iron sulfate, magnesium sulfate, copper sulfate or their mixtures, or their alums with common formula MIMIII(SO4)

.2
12H2O, where MI-Na,K,Pb,Cs,NH4, and MIII-Al,Cr,Fe,Mn.

EFFECT: higher efficiency.

2 tbl

FIELD: oil and gas extractive industry.

SUBSTANCE: method includes feeding water-isolating compound along tubing pipes, containing polyvinyl spirits and consisting of components forming an impenetrable zone in case of mixing in the bed, pressing it into bed, washing and exposure of well for forming of impenetrable zone, tubing column is lowered for 2-3 meters below perforation range, and into isolation range along tubing pipes hydro-repelling liquid is first pumped, in volume, exceeding volume of water-isolating composition in at least two times, water-isolating composition includes special liquid except from polyvinyl spirits, its pumping is performed in sequence - first goes polyvinyl spirits, then buffer liquid, special liquid, buffer liquid, repeating these operations until reaching required height of isolation interval and fixing of well-adjacent area, after that said pressing, washing of well and said polymerization exposure are performed.

EFFECT: higher efficiency.

1 dwg, 1 ex

Plugging mix // 2245989

FIELD: oil and gas production.

SUBSTANCE: plugging mix intended for cementation of oil, gas, and gas condensate wells under moderate and elevated temperatures contains 50-76% Portland cement, 20-40% finely ground quartz, and caustic magnesite powder.

EFFECT: reduced filtration and shrinkage of plugging mortar.

1 tbl

FIELD: oil and gas production.

SUBSTANCE: Portland cement-based composition contains, wt %: polymer 1-10, hardening accelerator 6-8. plasticizer 0.3-0.5, alumina cement 7-10, gypsum dihydrate and/or anhydrite 5-8, said polymer being selected from the group comprising: polyacrylamide, hydrolyzed polyacrylonitrile, polyvinyl alcohol, organosilicon liquid, latex and cationic bitumen emulsion, and said hardening accelerator being alkali or alkali-earth metal sulfates or chlorides.

EFFECT: improved properties, reduced shrinkage deformations, and under conditions resistance to fissuring.

2 cl, 2 tbl

FIELD: mining engineering, in particular improving of reservoir recovery.

SUBSTANCE: claimed composition contains (mass parts): resin 100; liquid curing agent (e.g., alkali solutions) 15.1-60; ammonium carbonate 0.1-9.9. Composition of present invention afford the ability to limit the water and sand inflow, to increase strength and permeability of formed reservoir.

EFFECT: improved reservoir recovery, increased turnaround time, reduced underground equipment in well.

2 tbl, 4 ex, 2 cl