Composition for degreasing of sheepskins

 

(57) Abstract:

Composition refers to the fur industry and can be used for degreasing fur and fur skins. The composition contains a nonionic surfactant, alkyldimethylbenzylammonium and perchlorethylene. The composition can improve the quality of degreasing and improve the elastic properties of sheepskin. table 2.

The invention relates to the fur industry and can be used for degreasing fur and fur sheepskin.

Known composition for degreasing fur sheepskin, containing the sodium salt of monoether sulfuric acid and the mixture of cetyl and oleic alcohol, sodium carbonate, formalin, hydrogen peroxide, it G3X-1 and water (SU authorship, 1098955, 23.06.84, CL C 14 C 1/08).

The disadvantage of this structure is that when it is used simultaneously with the oxidative and enzymatic degradation of wool fat is weakening due hairline with Koshevoy cloth sheepskin, which leads to teclast hair.

The closest analogue of the proposed technical solution is a composition for degreasing of sheepskins, including anion active surfactants (proxied hydrogen, nonionic surfactants and water. (SU authorship, 1002358, 07.03.83, CL C 14 C 1/08).

The disadvantage of this structure is that it has low degreasing ability in relation to the sheepskin, containing large amounts of fat in the hairline and the leather, resulting in lower quality sheepskin.

The technical result of the invention is to improve the quality degreasing of sheepskins, and the improvement of their elastic-plastic properties.

This result is achieved by the fact that the composition for degreasing of sheepskins, comprising nonionic surfactant and the organic compound further comprises alkyldimethylbenzylammonium, as well as organic compounds contains perchloroethylene in the following ratio, wt.%:

Nonionic surfactant - 80,0 - 90,0

Alkyldimethylbenzylammonium - 2,0 - 8,0

Perchlorethylene - Rest

A distinctive feature of the proposed structure is that the introduction of kationaktivnaya saw Catamine AB and an organic solvent can significantly improve the degree of degreasing of sheepskins, and does not allow remote fat again the components of the composition below the specified limits may result in incomplete removal of hair and the leather sheepskin. Increase the percentage of components above the proposed limits is impractical because of the further increase of the achieved effect does not occur.

The composition is prepared as follows.

In the reaction apparatus upload nonionic surfactants and alkyldimethylbenzylammonium (Ketamin AB) THE 9392-003-48482528-99, the resulting mixture with constant stirring heated for 20-25 min until a temperature of 50-60oC, and then injected into the reactor perchlorethylene THE 6-01-956-86 and all mix to obtain a homogeneous mass.

As the nonionic surfactants used Sintana DC-10, OP-10, Prevotella W-OF-100 and others.

Technology of application of the composition is as follows.

Party fur sheepskin, after soaking and wringing hair is subjected to the first degreasing the proposed composition concentration of 4-6 g/l at a temperature of 40-42oC for 30-45 minutes After cutting and meskene spend the second degreasing within 59-60 min proposed composition concentration of 5-6 g/L. Further processes and operations carried out by known processing techniques fur sheepskin.

Party fur sheepskin is treated as a party of fur, but concentration is of Ostapov for degreasing of sheepskins are presented in table. 1.

Qualitative indicators are processed sheepskins, in comparison with sheepskin on the prototype are presented in table.2.

Using the proposed structure allows to improve the quality of degreasing and elasto-plastic properties of fur and fur skins.

Composition for degreasing of sheepskins, comprising a nonionic surfactant and an organic compound, characterized in that it further comprises alkylbenzenesulfonic, as well as organic compounds contains perchloroethylene in the following ratio, wt.%:

Nonionic surfactant - 80,0 - 90,0

Alkyldimethylbenzylammonium - 2,0 - 8,0

Perchlorethylene - Rest

 

Same patents:

The invention relates to light industry and can be used in chemical processing of sheepskin raw materials and fur raw materials

The invention relates to the leather industry and can be used in making leather for various purposes

The invention relates to the processing of hides and skins of cattle and small cattle, which can be used for the production of leather for the uppers, and clothing and haberdashery

The invention relates to light industry and fur sub-sectors and can be used in Cyrano-dye production in dressing skins furs, with thin Koshevoy cloth, such as mink, sable, marten, etc

The invention relates to the leather industry and can be used in making leather for Shoe uppers from raw cattle

FIELD: fur industry, in particular, method for evaluating pickling quality of leather web in tanning of fur and sheepskin raw material.

SUBSTANCE: method involves providing testing on parallel groups of fur sheepskin after pickling on three topographic portions of sheep skin surface: skirt, spine and neck portions; processing samples of each group with acid-salt solution for 24 hours; withdrawing sheepskins of each group from acid-salt solution in predetermined time intervals; removing excessive liquid; placing said samples into tensile testing machine and stretching lengthwise of spine line by 40% relative to initial length thereof; holding samples in stretched state for 1 min and withdrawing from tensile-testing machine; leaving samples in free state for 10 min; determining residual elongation value in mm.

EFFECT: reduced time for determining quantitative pickling characteristic of skin web.

2 tbl, 2 ex

FIELD: fur industry, in particular, method for evaluating pickling quality of leather web in tanning of fur and sheepskin raw material.

SUBSTANCE: method involves determining quantitative pickling characteristic of leather web of semi-finished product by using time of solving thereof in alkaline solutions, said time depending on number and kind of intermolecular bindings destructed during pickling. Solving of collagen in alkaline solutions depends upon nature of preliminary acidic preparing procedure. Solving is provided in aqueous solution of potassium hydroxide having concentration of 150 g/l and temperature of 18-20 C. Derma solving time is found after preliminary thermal processing at temperature of 60-65 C during 1.5 hours. Method may be employed both in production of fur and sheepskin products and in fur processing.

EFFECT: wider operational capabilities and reduced time for determining quantitative pickling characteristic of skin web.

1 tbl, 1 ex

FIELD: leather industry.

SUBSTANCE: method comprises pickling, tanning, and neutralizing the semifinished item. During pickling and subsequent tanning, the picking liquid is provided with acetate sodium in amount of 0.2-0.5 % and, then, chromic tanner in amount of 1.5-1.8%. The tanning is carried out until the pH of the solution reaches 4.2-4.4.

EFFECT: enhanced quality of tanning.

2 tbl

FIELD: defatting of crude sheepskin-and-fur material.

SUBSTANCE: method involves treating crude material in bacterial suspension having lipolytic activity of 20-30 units/g and proteolytic activity of 2.5-3.5 units/g. Suspension contains product of total microorganism vital activity used in an amount of 4-8 g/dm3, synthetic surfactant used in an amount of 0.25-0.5 g/dm3, and prokaryotic crop of Pseudomonas sp. type used in an amount of 107-109 cells/cm3, water the balance. Treatment is conducted at temperature of 40±2 C during 45 min by providing mechanical actions, and liquid coefficient of 7-10.

EFFECT: improved quality of defatting sheepskins, improved elastoplastic properties and reduced level of toxic contamination of sewage water.

3 dwg, 4 tbl

FIELD: fur industry, in particular, process for pickling of sheepskin fur coats and raw fur material.

SUBSTANCE: method involves pickling fur sheepskins in solution such as sour-milk composition having titratable acidity of at least 300 T, lactic acid concentration of at least 25 g/dm3 and medium active reaction below 3.5; providing said process at temperature of 30±2 C during 16 hours at variable mechanical action, with liquid to acid ratio of 7, sodium chloride consumption of 20 g/dm3.

EFFECT: improved quality of fur sheepskins due to reduced curling of hair-covering and improved elastoplastic properties thereof.

4 tbl, 4 ex

FIELD: fur industry.

SUBSTANCE: invention is directed to processing fur sheepskin intended for manufacturing clothing, headgears, footwear parts and other fur items. Crude fur sheepskin of all preservation types is subjected to soaking, first degreasing, squeezing, haircutting, and fleshing according to known technology. Then fur sheepskin is subjected to additional processing in aqueous solution of sodium chloride (15-20 g/L) and nonionic surfactant composition (1-2 g.L) for 2-6 h at 30-32°C. After second degreasing and washing, pickle salting is carried out for 20-24 h. 4-6 hours after the beginning of pickle salting, processing solution is supplemented by 3-5 g composition of nonionic surfactants (1:1 mixture of Neonol AF 9-12 and syntamide 5). Finally tanning and greasing are performed.

EFFECT: improved performance characteristics fur sheepskin intermediate product.

2 cl, 1 tbl, 5 ex

FIELD: leather and fur industry.

SUBSTANCE: method envisages culturing of kefir fungal or kurungal ferment (obtained in amount 50%) on a nutrient medium, which medium is pasteurized skim milk for four first culturing days, pasteurized mixture composed of skim milk and fat-free curds whey on 6-14th days, and pasteurized fat-free curds whey on 15-18th days. Culturing is carried out for 18 days at 22±1°C and mechanical shaking twice a day for 15 min to give ferment with acidity 350-360°T. Ferment may be added to pasteurized cooled milk or to pasteurized curds whey in amounts 25% followed by fermentation at 22±1°C and acidity 350-360°T.

EFFECT: increased stability of ferment (double storage time), its acid-generating capability, and population autoregulation, increased activity to accumulate lactic acid by 2 1/2 times, and reduced restoration time by 4-6 h.

2 cl, 4 tbl, 6 ex

FIELD: leather industry.

SUBSTANCE: method involves pickling leather depilated hide with sodium chloride and sulfuric acid, addition of chrome tanning agent to the same bath in its consumption 0.5-0.6% of depilated hide mass as measured for chrome oxide, and chrome-plating is carried out for 2-4 h. Aliphatic dialdehyde is added to same bath in the concentration 3-6% of depilated hide mass, and treatment is carried out for 2-3 h wherein glyoxal or glutaraldehyde is used as dialdehyde. Invention provides enhancing thermal stability and strength properties of leather and can be used in tanning leathers for different designation and assortment.

EFFECT: improved tanning method.

2 cl, 1 tbl, 9 ex

FIELD: material processing.

SUBSTANCE: method provides degreasing and/or drying of animals' skins. According to method, skins, being subject to degreasing and/or drying, are brought in contact with one or more extractants. At least one dissolvent, selected from group consisting of dimethyl ether, methylal, dioxolane, diethyl ether and methyl ethyl ketone, is used as single dissolvent. Sheep, cows', goat's or pig's skins are subject to degreasing and drying. Process is carried out in stator or rotor reactor under pressure of 1-12 bar and at temperature between 5°C and 40°C.

EFFECT: improved efficiency of cleaning; improved ecological safety of process.

14 cl, 1 dwg, 4 ex

FIELD: chemistry.

SUBSTANCE: method involves degreasing sheepskin-fur raw material and can be used in fur production during degreasing of sheepskin-fur coat and fur raw material. Processing of the raw material is carried out in a degreasing bath containing a bacterial suspension, which has both lipolytic 50-60 units/gram and proteolytic 8-10 units/gram activity, with the total product of life activity of the microorganisms at a value of 5-6 g/dm3, synthetic surface-active substance - 0.5-1.0 g/dm3, catalase-positive procariotic culture of genus Erwinia sp. in the quantity 109-1010 cells/cm3 in the degreasing bath hydrogen peroxide is additionally added in the quantity 0.1-1.0 g/dm3, preliminarily dissolved in a tenfold amount of piped water. Processing is carried out at a temperature of 40±2°C, for 60 min., with some mechanical action from time to time and liquid crystallisation=10.

EFFECT: increase in quality of degreasing sheepskin and reduction in the level of toxic sewage production.

4 tbl, 4 ex

Up!